Product Name | Stainless steel rod |
Type: | Round bar |
Outer Diameter | 4-600mm (3/8"-25") |
Length: | 40-400mm,2000mm, 2500mm, 3000mm, 5800mm, 6000mm,12000mm, etc |
Standard: | ASTM,JIS, AISI, GB, DIN, EN |
Surface: | BA,2B,NO.1,NO.4,4K,HL,8K |
Application: | It is widely used in high-temperature and electric industry, medical devices, construction, chemistry, food industry, agriculture, and ship components. |
It also applies to food and beverage packaging, kitchen supplies, trains, aircraft, conveyor belts, vehicles, bolts, nuts, springs, and screen mesh etc. |
Certification: | ISO, SGS,BV |
Technique: | Forging and cold drawing |
Edge: | Mill Edge Slit Edge |
Quality: | SGS Inspection |
Grade (ASTM UNS) | 201,304,304L,321,316,316L,317L,347H,309S,310S,904L, |
S32205,2507,254SMOS,32760,253MA,N08926 |
Grade (EN) | 1.4301,1.4307,1.4541,1.4401,1.4404,1.4571,1.4438,1.4539,1.4547, |
1.4529,1.4562,1.4410,1.4878,1.4845,1.4828,1.4876,2.4858,2.4819 |
Main market: | Asia/Europe/South America |
20ft GP:5898mm(Length)x2352mm(Width)x2393mm(High) 24-26CBM |
40ft GP:12032mm(Length)x2352mm(Width)x2393mm(High) 54CBM |
40ft HC:12032mm(Length)x2352mm(Width)x2698mm(High) 68CBM |
SURFACE | CHARACTERISTIC | SUMMARY OF MANUFACTURING METHOD | APPLICATION |
NO.1 | Silvery white | Hot rolled to specified thickness | Do not need to have a glossy surface use |
lackluster |
NO.2D | Silvery white | After cold rolling, heat treatment and pickling are carried out | General material, deep material |
NO.2B | Gloss is stronger than No.2D | After No.2D treatment, the final light cold rolling is carried out through the polishing roller | The general material |
BA | As bright as a sixpence | No standard, but usually a bright annealed surface with high reflectivity. | Building materials, kitchen utensils |
NO.3 | Rough lapping | Grind with 100~200# (unit) strop tape | Building materials, kitchen utensils |
NO.4 | Intermediate grinding | Polished surface obtained by grinding with 150~180# strop abrasive tape | Building materials, kitchen utensils |
NO.240 | Fine lapping | Grinding with 240# strop abrasive tape | kitchenware |
NO.320 | Very fine grinding | Grinding was carried out with 320# strop abrasive tape | kitchenware |
NO.400 | The luster is close to BA | Use 400# polishing wheel to grind | General timber, building timber, kitchen appliances |
HL | Hairline grinding | Suitable particle material for hair stripe grinding (150~240#) with many grains | Building, construction material |
NO.7 | It's close to mirror grinding | Use a 600# rotary polishing wheel to grind | For art or decoration |
NO.8 | Mirror ultrafinish | The mirror is ground with a polishing wheel | Reflector, for decoration |
EN | ASTMUNS | C | N | Cr | Ni | Mo | COMPONENTV |
1.4301 | 304 | 0.04 |
| 18.1 | 8.3 |
|
|
1.4307 | 304L | 0.02 |
| 18.1 | 8.3 |
|
|
1.4541 | 321 | 0.04 |
| 17.3 | 9.1 |
| T0.24 |
1.455 | 347 | 0.05 |
| 17.5 | 9.5 |
| Nb0.012 |
1.4401 | 316,S31608 | 0.04 |
| 17.2 | 10.2 | 2.1 |
|
1.4404 | 316L,S31603 | 0.02 |
| 17.2 | 10.2 | 2.1 |
|
1.4406 | 316LN | 0.02 | 0.14 | 17.2 | 10.3 | 2.1 |
|
1.4429 | S31653 | 0.02 | 0.14 | 17.3 | 12.5 | 2.6 |
|
1.4571 | 316Ti,S31635 | 0.04 |
| 17 | 10.6 | 2.1 | T0.30 |
1.4438 | 317L,S31703 | 0.02 |
| 18.2 | 13.5 | 3.1 |
|
1.4539 | 904L,N08904 | 0.01 |
| 20 | 25 | 4.3 | 1.5Cu |
1.4547 | S31254,254SMo | 0.01 | 0.02 | 20 | 18 | 6.1 | Cu 0.8-1.0 |
1.4529 | N08926,Alloy25-6Mo | 0.02 | 0.15 | 20 | 25 | 5.5 | 1.ocu |
1.4462 | 2205,S32205,S31803 | 0.02 | 0.16 | 22.5 | 5.7 | 3 |
|
1.4410 | S32750,SAF2507 | 0.02 | 0.27 | 25 | 7 | 4 |
|
1.4501 | S32760 | 0.02 | 0.27 | 25.4 | 6.9 | 3.5 | W0.5-1.0-Cu0.5-1.0 |
1.4948 | 304H | 0.05 |
| 18.1 | 8.3 |
|
|
1.4833 | 309S,S30908 | 0.06 |
| 22.8 | 12.6 |
|
|
1.4845 | 310S,S31008 | 0.05 |
| 25 | 20 |
|
|
Carbon (C) : 1. Improve the deformation resistance and tensile strength of the blade;2. Enhance hardness and improve wear resistance.
Cr (Cr) : 1. Enhance hardness, tensile strength and toughness;2. Anti-wear and corrosion.
Cobalt (CO) : 1. Increase the hardness and strength so that it can withstand high temperature quenching;2. Used to enhance certain individual properties of other elements in more complex alloys.
Copper (Cu) : 1. Enhance corrosion resistance;2. Enhance wear resistance.
Manganese (Mn) : 1. Increase the quenchability, wear resistance and tensile strength;2. Removal of oxygen from molten metal by separate oxidation and separate vaporization;3. When added in large quantities, the hardness is enhanced, but the brittleness is improved.
Molybdenum (Mo) : 1. Enhanced strength, hardness, quenchability and toughness;2. Improve machinability and corrosion resistance.
Nickel (Ni) : 1. Enhance strength, hardness and corrosion resistance.
Phosphorus (P) : Enhanced strength, machinability and hardness.
2. When the concentration is too large, it is easy to crack
Silicon (Si) : 1. enhanced ductility;2. Increase the tensile strength;3. Removal of oxygen from molten metal by separate oxidation and separate vaporization.
Sulphur (S) : small amount used to improve machinability.
Tungsten (W) : Increases strength, hardness and toughness.
Vanadium (V) : Increases strength, hardness and seismic resistance.